I. Characteristics(1) The surface of the casting has linear or wavy lines, narrow and long, with development trend under external force;(2) Cold fissure-cracking where the metal is not oxidized;(3) Ho...
With the rapid development of the automobile industry, the design and production of the transmission housing, as a key component of automobile power transmission, has also received increasing attentio...
The reasons for blackened aluminum die casting parts after shot blasting are:1. The dust removal is not done in the equipment during shot blasting;2. There are oil stains, mold release and moisture on...